Matting agent dosage is one of the first numbers a formulator writes down and one of the last to be finalised. Ask how much silica a coating needs and the honest answer is: enough to hit the gloss target in your film, at your thickness, with your application method, and no more. This article explains what drives the right matting agent dosage, how to choose a sensible starting bracket, and how to recognise when you have gone too far in either direction.
Why there is no single matting agent dosage
Gloss reduction comes from particles disturbing the surface of the drying film. How much disturbance a given weight of silica produces depends on several things at once:
- Film shrinkage. High-solids and UV-curable films shrink little as they cure, so fewer particles are pushed up to the surface. Solvent-borne and waterborne films that lose a lot of volume on drying tend to concentrate particles near the surface and usually need less silica for the same gloss.
- Dry film thickness. Particles that are small relative to the film can sink into it and contribute little to surface roughness. Thicker films generally need either more silica or a coarser grade.
- Grade structure. Particle size, pore volume and oil absorption all change how much matting each gram delivers.
- Target gloss and measuring angle. Moving from 30 GU to 10 GU at 60° is a much bigger step than moving from 60 GU to 40 GU, and the last few gloss units are always the most expensive.
Because these factors interact, a dosage that works in one binder can be far off in another. Published figures should be read as a starting bracket for screening, not as a recipe.
Starting brackets by application
Our solution pages give a typical starting range for the lead grade in each application, expressed on total formulation:
- UV wood and panel coatings, VS3550U: 1–3 %.
- Waterborne clear wood topcoats, VS660: 2–4 %.
- Industrial and metal coatings, VS171S: 2–5 %.
- Deep matte finishes, VS361C: 2–5 %.
- Leather and synthetic leather, VS131A: 2–5 %.
- Flexible and soft-touch coatings, VS341S: 2–5 %.
Treat each range as a bracket rather than a target. Screen three loadings that span it, measure gloss, and interpolate to your specification. If the target falls outside the bracket, that is a signal to revisit the grade rather than simply to keep adding powder. You can compare the full range of grades on the products page or narrow the field with the grade selector.
Be clear about the basis: total formulation or solids
A frequent source of confusion is the basis on which dosage is quoted. Our recommendations are on total formulation, but many laboratories work on binder solids or on resin solids, and the difference is large. In a waterborne system at around 35 % solids, 3 % on total is roughly 8–9 % on solids; in a 100 %-solids UV system the two figures are the same.
When transferring a formulation between sites, or comparing your results with a supplier's guidance, write down the basis next to every number. It also helps to record the dosage as a volume fraction of the dry film where possible, because that is what actually governs surface texture.
How grade properties change the amount you need
The technical data sheets give the parameters that explain why two grades at the same weight produce different gloss:
- Particle size. Coarser grades, such as the industrial C-series VS381C (8.0–8.3 µm) and VS391C (9.0–9.5 µm), generally reach a given gloss at lower addition levels than fine grades, at the cost of a rougher feel and a greater risk of visible texture in thin films.
- Pore volume. Higher pore volume generally means more efficient gloss reduction at a given particle size, and a greater influence on viscosity. Most of our coatings grades sit between 1.3 and 1.8 mL/g.
- Oil absorption. Oil absorption by the DBP method ranges from 140–160 mL/100 g for VS3550U to 340–360 mL/100 g for VS3851. Higher values mean more matting efficiency and more thickening per gram, which can cap how much you can add before application properties suffer.
- Surface treatment. Treated grades, indicated by a higher loss on ignition, usually disperse more easily and have less impact on viscosity, which can allow higher loadings in systems that are sensitive to rheology.
The practical lesson is that comparing grades at the same dosage tells you little. Compare them at matched gloss, as described in our article on measuring matting efficiency, and then look at what each grade costs you in viscosity, clarity and feel at that loading.
Signs you have added too much
Gloss is the easy variable to correct; the side effects of overloading are not. Watch for:
- Viscosity rise and poor flow, especially with high oil absorption grades, leading to orange peel, brush marks or the need for extra solvent or water.
- Loss of clarity in clear coats over dark wood or coloured substrates, seen as a grey or milky cast.
- Burnishing and polishing, where rubbed areas become glossier because the film surface is dominated by loosely bound particles.
- Weaker film properties, including reduced scratch, chemical or water resistance and, in flexible coatings, cracking on elongation.
- Settling and hard sediment in storage as the pigment volume rises.
If you need more than the upper end of the bracket to reach the target, it is usually better to move to a more efficient or coarser grade than to keep raising the loading.
Signs you have added too little
Underdosing is less damaging but causes its own problems. Gloss may meet specification on a thick laboratory drawdown yet rise on a thinner production film. Small changes in film thickness, drying conditions or application method then produce visible gloss variation between panels or batches. A formulation sitting right at the edge of its gloss specification is fragile; aim for a loading that keeps you comfortably inside it across the film thickness range your customers actually apply.
A practical dosage-setting routine
- Fix the grade first from the constraints that loading cannot correct: clarity, surface texture, feel and dispersion stability.
- Prepare a ladder of three loadings spanning the starting bracket for your application, using the same dispersion procedure for each.
- Apply at production film thickness and with a method as close to production as possible, then cure or dry under realistic conditions.
- Measure gloss at the angle in your specification, and at 85° as well for low-gloss targets, then interpolate to the target.
- Check the side effects at the chosen loading: viscosity, clarity, rub and burnish resistance, and storage stability.
- Confirm at the extremes by repeating at the thinnest and thickest film you expect in the field.
Record the result with the basis, film thickness and gloss angle, so the number remains meaningful when someone else picks up the formulation.
Getting help with your starting point
A good matting agent dosage is the lowest loading that holds your gloss target reliably across real-world film builds without compromising the other properties of the coating. If you would like help choosing a grade or a starting bracket for a specific system, contact our technical team with your binder type, application method, film thickness and target gloss.