Silica Flatting Agents Explained: Same Job, Different Name
Flatting agent and matting agent name the same additive. Here is where the two terms come from, the other labels you will meet on specifications, and how to translate a flatting brief into a silica grade you can screen.
If you have ever compared a US paint formulation with a European or Asian datasheet, you have probably met both terms: silica flatting agent and silica matting agent. They describe the same additive doing the same job — a fine, porous silica that lowers the gloss of a dried coating film. The difference is vocabulary, not chemistry. This article explains where the two terms come from, the other names you will see on specifications and RFQs, and how to turn a “flatting agent” request into a grade specification you can actually screen.
Flatting agent or matting agent: one function, two vocabularies
A flatting agent and a matting agent are additives that reduce specular gloss by roughening the surface of the cured film on a microscopic scale. When the product is silica, the material is normally a synthetic amorphous silica (CAS 7631-86-9), most often made by precipitation and supplied as a micronised powder with a controlled particle size and pore structure.
Nothing about the powder changes with the name. A grade sold as a flatting agent in one market and as a matting agent in another has the same particle size, surface area, oil absorption and surface treatment. What matters to the formulator is those properties, not the label on the bag.
Why the coatings industry uses both terms
“Flatting” comes from the language of sheen. Architectural paint in North America has long been sold by sheen name — flat, matte, eggshell, satin, semi-gloss, gloss — and an additive that pushes a paint toward “flat” became a flatting agent. You will still find the term in US formulation guides, older technical literature and phrases such as “flatting efficiency”.
“Matting” is the more common term in Europe and Asia and across industrial, wood, plastic and leather coatings, where the finish is specified by a measured gloss value rather than a sheen name. In international trade the two are used interchangeably, and many buyers search for both.
A practical consequence: sheen names are not standardised. One company’s “flat” may be another’s “matte”, and the gloss ranges behind each name vary by manufacturer and region. If a brief only says “flat”, ask for a number.
Other names you will meet on datasheets and RFQs
Besides flatting and matting agent, the same function appears under several labels:
- Flattening agent or deglossing agent — descriptive variants, common in translated documents.
- Delustrant or delustering agent — more usual in fibres and textiles, sometimes used for coatings.
- Synthetic amorphous silica, precipitated silica or SiO2 — chemical descriptions that may appear on an SDS or customs paperwork instead of a functional name.
- Treated or untreated silica — whether the surface carries an organic treatment (often wax or polymer) to help dispersion, suspension or feel.
Not every gloss reducer is silica. Waxes, polymer beads and some fillers also lower gloss, by different mechanisms and with different side effects on clarity, feel and durability. When a specification says “flatting agent” without naming the chemistry, confirm whether silica is intended before you substitute.
What a silica flatting agent actually does in the film
As the coating dries and shrinks, silica particles near the surface create a fine micro-roughness. Incoming light is scattered in many directions instead of being reflected at a single angle, so the gloss meter reads lower. Three properties set how well a grade does this:
- Particle size — larger particles generally flatten more efficiently but can make the surface feel rougher and reduce clarity; finer particles give smoother, more refined finishes.
- Pore volume and surface area — higher pore volume usually means more gloss reduction at a given particle size, along with a greater influence on viscosity.
- Surface treatment — affects ease of dispersion, settling behaviour and compatibility with the binder.
For a fuller explanation of the mechanism and of how precipitated silica is produced, see our earlier guides in the news section.
Translating a flatting request into a grade specification
Whatever the brief calls the additive, the useful questions are the same:
- Target gloss and geometry. A value in gloss units at 60°, and for very low sheen also at 85°, where differences between flat finishes become easier to measure.
- System. Waterborne, solvent-borne or UV-curable; clear or pigmented; and the resin type.
- Application and film build. Spray, roller, curtain or brush, and the dry film thickness — thin films need finer particles.
- Constraints. Clarity, feel, scratch resistance, viscosity limits and storage stability.
Those answers point to a particle route. As examples from the Vistamatt technical data sheets: for high-clarity waterborne clear wood, VS660 (5.0–5.3 µm) is the lead grade; for UV spray, the fine VS141S (3.8–4.0 µm); for industrial and metal finishes, VS171S (7.0–7.5 µm), with coarser C-series grades such as VS391C (9.0–9.5 µm) held for lower gloss targets; and for deep matte surfaces, VS1650A (6.2–6.5 µm). Across the range, BET surface area runs from 170 to 600 m²/g, which is why grades with similar particle size can still behave differently in viscosity and flatting efficiency.
If you are replacing an existing flatting agent, the TS 100 alternative page and the other comparison pages show how Vistamatt grades are matched on particle route and application rather than claimed as identical products. The grade selector narrows the range by application and gloss window.
Common misunderstandings
- “Flat” is not a number. Agree a gloss value and measuring angle before screening, or two labs can disagree about whether the target was met.
- More is not always flatter in a useful way. Raising the dosage lowers gloss but also raises viscosity and can affect clarity, feel and film properties. Changing particle size or pore volume is often a better lever.
- Gloss at 60° does not tell the whole story. Two panels at the same 60° value can look different at a low viewing angle. Check 85° sheen for flat finishes.
- Dispersion matters. An under-dispersed flatting agent can leave seeds or uneven gloss; an over-dispersed one may lose efficiency. Keep the dispersion step constant when comparing grades.
Where to start
Treat the name as a synonym and focus on the specification. Define the gloss target, system and film build, pick a particle route from the data sheet, and screen a lead grade against a comparison grade in your own formulation at matched gloss. Vistamatt ships samples for evaluation in your system and issues a batch CoA with every shipment. Contact us with your resin type, gloss target and application method, and we will suggest a screening pair.