Matting Agent Pore Volume: Getting More Matte per Gram

At the same particle size, the more porous silica usually matts harder per gram. Here is what matting agent pore volume measures, why it drives efficiency, what it costs in viscosity, and how to use it when shortlisting grades.

Why matting agent pore volume matters

Two silica grades can share the same d50 and still give different gloss at the same loading. Much of that difference comes down to matting agent pore volume: the internal void space inside each porous silica particle, reported in mL/g. Pore volume decides how much particle volume, and therefore how many particles, you get from each gram you weigh into the batch. Once particle size is chosen for the film, it is the next property to read on a datasheet if you want more matte per gram.

This article explains what pore volume measures, why it drives matting efficiency, what it costs in viscosity and handling, and how to use the published values for the Vistamatt range when shortlisting grades.

What pore volume measures

Precipitated and gel-type silica matting agents are not solid spheres. Each particle is a rigid network of fused primary silica particles with a large amount of open space between them. Pore volume expresses that space per unit mass. On the Vistamatt technical data sheets it is measured by nitrogen desorption and reported in mL/g; across the published range it runs from about 1.2 to 1.9 mL/g.

Three other datasheet values are closely related and should be read together with it:

  • BET surface area (m2/g) describes how finely that pore space is divided. The same pore volume can be made of a few wide pores or many narrow ones.
  • Oil absorption (DBP, mL/100 g) reflects how much liquid the powder takes up before it wets out. It generally rises with porosity, but surface treatment and the space between particles also affect it.
  • Loose bulk density (g/cm3) tells you how much space the powder occupies in the bag. Highly porous powders are light and voluminous.

From pore volume to particles per gram

A silica matting agent works by putting particles at the surface of the drying film. As solvent or water leaves and the film shrinks, those particles create micro-roughness that scatters reflected light, and gloss falls. What matters for that effect is the number and volume of particles present, not their mass.

Pore volume converts mass into volume. The solid silica skeleton is dense, roughly 2.2 g/cm3, so its own contribution per gram is small (about 0.45 cm3). The pores add the rest. As an idealised illustration:

  • At a pore volume of 1.3 mL/g, one gram of silica occupies roughly 1.75 cm3 of particle volume.
  • At 1.8 mL/g, the same gram occupies roughly 2.25 cm3.

At equal particle size, that is close to 30% more particles per gram from the higher-porosity grade. This is the core of why the Vistamatt TDS notes that higher pore volume generally means more efficient gloss reduction at a given particle size. In practice the gain is smaller or larger depending on how well the particles are dispersed, how much the film shrinks and whether some pore structure is lost during grinding, so treat the arithmetic as a direction, not a prediction.

The cost of porosity: viscosity, wetting and handling

Pore space does not stay empty in a coating. It absorbs binder, solvent or water, which is why porous silica raises viscosity and why the TDS describes higher pore volume as having a greater influence on system viscosity. Expect the following when moving to a more porous grade:

  • Higher viscosity at equal loading. Partly offset because you may need a lower loading for the same gloss. Compare at matched gloss, not matched percentage.
  • Longer wetting time. Air has to be displaced from the pores. Add the silica slowly under agitation and allow time before judging viscosity or gloss.
  • Dusty, bulky powder. Lower bulk density means more volume per kilogram in the bag and in the mixing vessel.
  • Sensitivity to over-dispersion. A very open structure can be broken down by excessive shear, shifting the particle size finer and pushing gloss up. Disperse to a consistent end point rather than "as long as possible".

In solvent-free or high-solids systems with little shrinkage, extra porosity may raise viscosity faster than it improves matting. In waterborne and conventional solvent-borne clear coats, where shrinkage is substantial, efficiency per gram is usually the larger benefit.

Pore volume, surface area and pore size

Pore volume and BET surface area together give a rough picture of pore size. Assuming simple cylindrical pores, average pore diameter is about four times pore volume divided by surface area. Applied to the published ranges:

  • A typical Vistamatt grade with pore volume of 1.6–1.8 mL/g and BET of 250–280 m2/g works out to pores in the region of 25 nm.
  • VS3550U, with BET of 500–600 m2/g and pore volume of 1.2–1.5 mL/g, works out to roughly 10 nm: a much finer pore structure. Its oil absorption (140–160 mL/100 g) is also the lowest in the range.

The point is not the exact number but the pattern: high surface area does not automatically mean high pore volume or high oil absorption. Read the three values together before assuming how a grade will behave in your binder.

Reading the Vistamatt range by pore volume

The production specification ranges on tds.html show how pore volume is used across the portfolio:

  • Higher pore volume (1.6–1.8 mL/g and above): most waterborne clarity grades (VS351C, VS651, VS660, VS1531D, VS6550), the industrial C-series (VS361C, VS381C, VS391C), the deep-matte grade VS1650A, the UV grades VS641, VS370U and VS6907, and VSKD721 (1.6–1.9 mL/g) for leather.
  • Moderate pore volume (about 1.3–1.6 mL/g): soft-touch and leather grades such as VS331S, VS341S, VS370T and VS3851, and the UV grade VS141S.

Two comparisons in the data are useful because they separate pore volume from particle size:

  • VS141S and VS641 are both close to 4 µm (3.8–4.0 and 3.8–4.2 µm) and both used in UV wood and panel coatings, but VS641 carries a higher pore volume (1.6–1.8 vs 1.3–1.6 mL/g). At similar particle size, it is the candidate to screen first when matting efficiency per gram is the priority.
  • VS361C, VS381C and VS391C share the same pore volume, BET and oil absorption ranges and differ in particle size (6.2–6.5, 8.0–8.3 and 9.0–9.5 µm). Here pore volume is held constant and particle size is the variable, matched to film thickness.

Moderate pore volume is not a weakness. In soft-touch and flexible coatings, particle size, surface treatment and haptics often matter more than the last increment of efficiency, which is why those grades are built differently. For premium matte finishes targeting below 10 GU at 60°, see the deep matte surfaces grades.

A practical way to screen for efficiency

  1. Fix particle size first. Choose candidates whose d50 suits your dry film thickness, then compare pore volume within that group.
  2. Build a ladder. Make three or four loadings per grade and plot 60° gloss (and 85° for low-gloss targets) against loading.
  3. Read efficiency at matched gloss. Note the loading each grade needs to hit your target, then record viscosity at that loading.
  4. Hold the process constant. Same dispersion equipment, time, film build, flash-off and cure for every panel.
  5. Check the side effects. Clarity on dark substrates, settling after storage and recoat behaviour at the chosen loading.

The grade that needs the least silica to reach gloss is not always the winner: the viscosity at that loading and the appearance of the film decide whether the efficiency is usable.

Key takeaways

  • Pore volume converts weight into particle volume. At equal particle size, higher pore volume means more particles per gram and usually more matting per gram.
  • Porosity costs viscosity and wetting time; compare grades at matched gloss, not matched loading.
  • Read pore volume together with BET, oil absorption and particle size; none of them tells the whole story alone.
  • Within the Vistamatt range, pore volume runs from about 1.2 to 1.9 mL/g; most efficiency-focused grades sit at 1.6–1.8 mL/g.

To narrow the shortlist for your system, use the grade selector or ask for samples and a grade-specific TDS.

Grade recommendations are a starting point for screening. Final suitability, dosage and performance must be verified in the customer's own resin system, at the target gloss and under actual process conditions.