jackson@vistamatt.com +1 619 558 6563 Technical documents Request a sample

Home/News/Technical Insight

Organically Treated Silica: Better Settling, Feel and Scratch Resistance

Organic treatment does not change how silica lowers gloss, but it changes how the particles settle, how the film feels and how the surface handles abrasion. Here is where organic treated silica helps, what it can cost, and how to screen it fairly.

An organic treated silica matting agent is synthetic amorphous silica whose particle surface has been partly covered with an organic layer after manufacture. The layer does not change how the silica lowers gloss: particles near the surface of the drying film still create the micro-roughness that scatters light. What it changes is how the particles behave around that job, in the can, on the dispersion line and in the cured film. For formulators working on deep matte, soft feel or handled surfaces, those side effects often decide whether a grade passes. This article explains what organic treatment does, where it helps most, what it can cost, and how to screen a treated grade against an untreated one fairly.

What organic treated silica means

Every silica matting agent starts as a porous particle covered in silanol (Si–OH) groups. Those groups are polar and reactive: they bond to each other, to water and to polar parts of the formulation. That activity is behind several familiar effects of untreated silica, including viscosity build and the firm sediment it can form in storage.

Organic treatment covers part of that surface. In the industry the term spans several chemistries: waxes, polymer treatments and other organic modifiers applied to the silica. On cross-reference pages you will see the range reflected in how incumbent grades are described, for example as wax-treated amorphous silica, organic treatment on the ED 30 alternative page, or as an organically treated micronized silica gel, for radiation cure on the RAD 2005 alternative page. Wax treatment is one member of the family; an earlier article compared wax-treated and untreated silica directly. Here the focus is on the three outcomes most often specified when an organically treated grade is chosen: settling, feel and scratch resistance.

Better settling behaviour

Silica is denser than any liquid binder, so some settling in storage is normal. The question is what the sediment looks like. Untreated particles, with free silanols on their surfaces, can draw together and pack into a hard layer that is difficult to stir back in. Treated particles interact less with each other and tend to form a softer, looser sediment.

That difference matters most where loadings are high. Deep matte is the clearest case: reaching a very low gloss in a clear system can require 5–8 % silica, as described in the deep matte how-to. At that level, a hard-packing grade can turn a storage test into a reformulation project. A treated grade does not remove the need for an anti-settling package, but it often makes the package’s job easier.

Practical checks:

  • Store samples at elevated temperature alongside room temperature and inspect the sediment, not just the volume.
  • Record how much stirring is needed to restore a uniform paint, and re-measure gloss after re-dispersion.
  • Test the full batch size you intend to ship; small jars can settle differently from drums.

Surface feel

Feel has become a specification in its own right for furniture, interior trim, consumer electronics and leather. A matte film can measure perfectly on a gloss meter and still feel dry, draggy or powdery. Organic material at the particle surface lowers friction where the particles meet the film surface, which is why treated grades are common in finishes where the hand is judged as carefully as the gloss.

Feel is still a system property. Particle size, film build, binder hardness and the slip additive package all contribute. The deep matte test list on the premium deep matte surfaces page asks for a surface that is “fine and soft; free of drag or powdery feel”, and that is best judged by side-by-side panels touched blind, not by a single number.

Scratch, mar and burnish resistance

Matte films are vulnerable to two kinds of damage. Scratching or marring can leave white marks where the surface is disrupted. Burnishing does the opposite: rubbing flattens or removes the surface roughness and leaves glossy patches. Both show up more on deep matte, because the contrast with the surrounding film is larger.

An organic layer can help on both counts by lowering friction at the surface and changing how particles sit in the binder. It is not a substitute for a hard, well-cured binder, and results vary widely by system. Treat scratch and mar as a test, not an assumption: abrade treated and untreated panels the same way and look for white marking, gloss change and visible damage.

What treatment can cost

Organic treatment solves some problems and can introduce others. Check these before switching:

  • Recoat and intercoat adhesion. Organic material at the surface can reduce adhesion of a following coat. Test it wherever a finish is sanded and recoated or is part of a multi-coat build.
  • Waterborne compatibility. Waterborne systems are more sensitive to wetting and dispersion, and some treatments designed for solvent chemistry underperform in water. A grade that works in a solventborne system should not be transferred directly.
  • Cure interaction. In sensitive cure chemistries, an extra organic component is one more variable to check.
  • Matting efficiency. Depending on the system, a treated grade may need a different loading from an untreated grade of similar size to reach the same gloss. Compare at matched gloss, not matched loading.

Reading treatment level on the datasheet

Datasheets rarely describe treatment chemistry in detail, but loss on ignition (LOI) gives a useful signal. Calcination burns off bound organics, so on the Vistamatt technical data sheets a higher LOI indicates a more heavily treated surface. Many grades sit around 4.4–4.6 %, while others run well above that, such as VS660 at 8.25 %, VS1650A at 10.46 %, VS3550U at 12.65 % and VS6907 at 14.35 %.

The deep matte range shows why this is a useful lever. VS1650A and VS361C share the same particle size (6.2–6.5 µm), BET surface area (250–280 m²/g) and pore volume (1.6–1.8 mL/g), with oil absorption of 270–290 and 280–300 mL/100 g respectively. Their LOI is very different: 10.46 % for VS1650A against 4.46 % for VS361C. Running the two in the same round isolates the effect of surface treatment from the effect of particle size, which is rarely possible with grades from different families.

Two cautions apply. LOI also includes bound water and other volatiles, so it indicates treatment level rather than measuring it. And two grades with similar LOI can carry different treatments. If the treatment type matters to your system, ask for it to be confirmed in writing for the specific grade before you formulate.

How to screen an organically treated grade

  1. Fix the particle route first. Choose particle size from your clarity and texture constraints. The grade selector gives a starting point by application.
  2. Pair treated and untreated at the same size. On the deep matte route, VS1650A is listed as the primary route for first screening and VS361C as the grade that balances matting depth against surface refinement.
  3. Bracket the loading. Screen three loadings and interpolate to your gloss target, then compare grades at matched gloss.
  4. Test what treatment is meant to change. Settling after hot storage, blind touch panels, and scratch and mar on cured films.
  5. Test what treatment can break. Recoat adhesion, viscosity at application solids, defoaming and cure.

Run this against your current control in your own binder and at production film build. Organic treatment is a selection variable to be screened, not a box to tick, and the result in your system is the only one that counts.

Grade recommendations are a starting point for screening. Final suitability, dosage and performance must be verified in the customer's own resin system, at the target gloss and under actual process conditions.